LDPE film grade can be categorized into several groups – general purpose film, highly transparent film, heavy-duty film, shrinkage film and casting film. These products have excellent physical and mechanical performence, good chemical stability and electric insulation, low permeability to vapor, and excellent processability. Films produced using these resins has excellent transparence and aging resistance.
LDPE film grade is principally used in the production of blowmolding packaging film, agricultural film and can be blended with linear low-density polyethylene (LLDPE) to produce modified PE. In addition, it can be used for heat shrinkable packaging film, laminated film, freezing film, medical packaging, multi-layer coextrusion film, heavy-duty packaging film, pipe coatings, cable sheathing, lining and high-end chemical foaming.
The resin is packaged in internally film-coated polypropylene woven bags. The net weight is 25Kg/bag. The resin should be stored in a drafty, dry warehouse and away from fire and direct sunlight. It should not be piled up in the open air. During transportation, the product should not be exposed to strong sunlight or rain and should not be transported together with sand, soil, scrap metal, coal or glass. Transportation together with toxic, corrosive and flammable substance is strictly prohibited.
Grades | LD100AC | LD163 | 2102TN00 | 2102TN26 | 2100TN00 | |
MFR | g/10 min | 2 | 0.31 | 2.40 | 2.40 | 0.30 |
Density | 23°C, g/cm3 | 0.9225 | 0.9220 | 0.920 | 0.920 | 0.920 |
Haze | % | – | – | 7 | – | 14 |
Tensile Strength | MPa | 9 | 14 | 12 | 11 | 14 |
Elongation at break | % | 500 | 500 | 550 | 450 | 550 |
Grades | LD605 | N150 | N210 | S030 | N220 | |
MFR | g/10 min | 6.5 | 1.5 | 2.1 | 0.3 | 2.2 |
Density | 23°C, g/cm3 | 0.9230 | 0.919 | 0.921 | 0.920 | 0.922 |
Haze | % | – | 24 | 16 | 16 | 16 |
Tensile Strength | MPa | 8 | 12.5 | 11 | – | 15 |
Elongation at break | % | 100 | 550 | 550 | – | 500 |
Grades | Q210 | Q281 | Q281D | Q400 | 951-000 | |
MFR | g/10 min | 2.1 | 2.8 | 2.8 | 4.0 | 2.17 |
Density | 23°C, g/cm3 | 0.921 | 0.924 | 0.925 | 0.923 | 0.92 |
Haze | % | 10 | 10 | 6.1 | 10 | 9 |
Tensile Strength | MPa | 11 | 11 | 14.5 | 16 | 8 |
Elongation at break | % | 550 | 550 | 620 | 450 | 400 |
Grades | 951-050 | 2426K | 2426H | 2520D | |
MFR | g/10 min | 2.17 | 4.0 | 1.9 | 0.3 |
Density | 23°C, g/cm3 | 0.92 | 0.926 | 0.923 | 0.924 |
Haze | % | 9 | 10 | 8 | 11 |
Tensile Strength | MPa | 8 | 18 | 15 | 11 |
Elongation at break | % | 400 | 550 | 600 | 600 |
Grades | QLT04 | QLF39 | |
MFR | g/10 min | 3.0 | 0.75 |
Density | 23°C, g/cm3 | 0.920 | 0.920 |
Haze | % | 10 | |
Tensile Strength | MPa | 6 | 6 |
Elongation at break | % | 550 | 550 |